Titanium Alloy Grade 7 with 0.1% palladium is similar to Grade 2, but with improved resistance to general and localized crevice corrosion in a wide range of reducing acid environments, including chlorides, and where low pH and high temperatures above 180ºF (83ºC) to 500ºF (260ºC) are prevalent.
Standard Specification: ASTM B338, ASTM B861, ASTM B862, GB/T3625
| Standard | Werkstoff No. | UNS | 
| Titanium Alloy Grade7 Ti-0.2Pd | 3.7235 | R52400 | 
Technical Data Sheet
| `Chemical Composition | |||||||
| Weight % | Ti | Pd | C | Fe | N | O | H | 
| Titanium Alloy Grade7 Ti-0.2Pd | Balance | 0.12~0.25 | 0.08 | 0.3 | 0.03 | 0.25 | 0.015 | 
Typical Mechanical Properties (Tensile Requirements)
| Material | Tensile Strength, min | Yield Strength (0.2% Offset) min or range | Elongation in 4D,min% | Reduction of Area Min % | ||
| ksi | MPa | ksi | MPa | |||
| Titanium Alloy Grade7 Ti-0.2Pd | 50 | 345 | 40 | 275 | 20 | 30 | 


Ti-6Al-4V ELI Alloy is the most widely used titanium alloy of the alpha-plus beta class, and is also the most common of all titanium alloys. This modification incorporates extra low int
Titanium Alloy Grade5 Ti-6Al-4V Ti-6Al-4V alloy is the most widely used titanium alloy of the alpha-plus-beta class,and is also the most common of all titanium alloys. The alloy is castable and is&nbs
Titanium Alloy Grade 3 is “unalloyed” titanium offering improved strength,moderate ductility, and ASME Code design allow ables. The material is readilyweld able. This material is very corros
Titanium Alloy Grade 2 is “unalloyed” titanium offering an excellent balanceof strength and ductility. The material has good toughness and is readilyweldable. This material is very corrosion resistant